Cast iron electrodes

MONEL

Electrode with monel-core wire is suited for cold welding of grey cast iron and other types of cast iron. It is suitable for repair purposes. By using small electrode diameters heat input should be kept low. The weld metal is easily machinable.

 

MONEL C

Electrode with monel-core wire is suited for cold welding of grey cast iron and other types of cast iron. It is suitable for repair purposes. By using small electrode diameters heat input should be kept low. The weld metal is easily machinable. Electrode contents no Ba components.

 

SUPER Ni

Electrode with pure Ni-core wire for cold welding of grey  and malleable cast iron also suitable for joining them with steel. Suitable for repair purposes, repair of broken parts, building up missing parts and correction of machining errors, joining cast iron for rectification of castings. The weld material is soft and easy machinable We suggest cold impact forging to achieve stress relieving. By using small electrode diameters heat input should be kept low. Ground material should be clean. For scoring we suggest our electrode Sekator 2 B or Sekator 2 A, grinding is not recommended.

 

CAST Ni

Electrode with pure Ni-core wire for cold welding of grey and malleable cast iron without preheating, for repair purposes, also suitable for joining them with steel, copper and monel. Suitable for repair purposes, repair of broken parts, building up missing parts and correction of machining errors, joining cast iron for rectification of castings. The weld metal is soft and easily machinable. We suggest cold impact forging to achieve stress relieving. By using small electrode diameters heat input should be kept low. Ground material should be clean. For scoring we suggest our electrode Sekator 2B or Sekator 2A, grinding of is not  recommended.

 

CAST NiC 

Nickel electrode for joining and surfacing of grey cast iron. Stable arc with clear bead appearance. Electrode provides crack resistant bead without pore formation. Chipforming machining processes can be used. Weld induced stresses can be reduced by hammer peening. Repair and recovery of broken or worm parts made of grey and malleable cast iron. Filling of voids and blowholes, machining errors. Joining of grey cast iron to steel.

 

CAST NiFe

Electrode with Ni-Fe alloyed core wire for cold welding nodular, grey and malleable cast iron, also suitable for the rectification an repair of these grades and joining them with steel. Tensile strength is higher than tensile strength of Ni electrodes. Welding joints are suitable for after treatment. By using small electrode diameters heat input should be kept low. The weld metal is stronger and more resistant to impurities than nickel-cored type.

 

CAST NiFe C 

Electrode with Ni-Fe alloyed core wire for cold welding nodular, grey and malleable cast iron, also suitable for the rectification an repair of these grades and joining them with steel. Tensile strength is higher than tensile strength of Ni electrodes. Welding joints are suitable for after treatment. By using small electrode diameters  heat input should be kept low. The weld metal is stronger and more resistant to impurities than nickel-cored type. Electrode contents no Ba components.

 

CAST NiFe B 

Electrode with Ni-Fe bimetal core wire for cold welding nodular, grey and malleable cast iron, also suitable for the rectification an repair of these grades and joining them with steel. Tensile strength is higher than tensile strength of Ni electrodes. Welding joints are suitable for after treatment. By using small electrode diameters heat input should be kept low. The weld metal is stronger and more resistant to impurities than nickel-cored type. It has better welding characteristics than Cast NiFe electrode.

 

CAST NiFe10

Electrode with pure Ni-core wire for cold welding of cast iron and joining cast iron to steel. Specially suited for welding spheroidal cast iron. Electrode is more resistant to impurities and has good weldability on oily cast iron. This electrode can be used for combination welding with CAST Ni electrode. By using small electrode diameters heat input should be kept low. To avoid overheating the seams should not be longer than 10 times the electrode diameter. For scoring we suggest our electrode Sekator 2 B or Sekator 2 A, grinding of is not recommended. Welding joints are suitable for after treatment.

 

CAST Fe

Electrode with iron core wire for cold welding repair on poorly weldable or slag containing old cast iron, nodular, grey and malleable cast iron, where Ni base electrodes do not give a solid bond. It is specially suitable for buffering layers before welding them with Cast Ni, Cast NiFe  welding consumables. The weld deposit can be machined by grinding. It is not corrosion resistant.

 

SL 250

Thick coated electrode with  mild steel core wire and 200% recovery suitable for welding large sections of preheated grey cast iron up to the quality of SL 25-type of material. Suitable for reparations of moulds. Weld material is machinable after slow cooling.  

PRODUCTS EN ISO 1071 DIN 8573 A-5.15
MONEL EC NiCu-1 E NiCu G12 E NiCu-B
MONEL C EC NiCu-1 E NiCu G13 E NiCu-B
SUPER Ni EC NiCu-1 E Ni BG12 E Ni-Cl
CAST Ni EC NiCu-1 E Ni BG12 E Ni-Cl
CAST Ni C EC NiCu-1 E Ni BG13 E Ni-Cl
CAST NiFe EC NiFe-Cl-1 E NiFe BG12 E NiFe-Cl
CAST NiFe C EC NiFe-Cl-1 E NiFe BG13 E NiFe-Cl
CAST NiFe B EC NiFe-Cl-1 E NiFe BG12 E NiFe-Cl
CAST NiFe 10 ~E Ni BG12 ~E Ni-Cl
CAST Fe EC St 1 ~E NiFe BG13 ~E St
SL 250 EC FeC-2-7 E (FeC-2) BG 49 /

Renata Hočevar